Used to overlay mild and low alloy steels
Key Features
- Preheat and inter-pass temperatures of 300ยฐF (150ยฐC) or greater are recommended during welding
- Post-weld heat treatment should not exceed 1150ยฐF (620ยฐ C) as higher temperatures may result in hardening
- Q2 Lot - Certificates showing actual wire chemistry available online